H.C. Starck Ni-SA 625 Nickel Super Alloy

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Ni-SA 625 Nickel Super Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ni-SA (Nickel Super Alloys) prevents high temperature corrosion, pitting and crevice corrosion and oxidation for chemical processings with high mechanical stresses, heat exchanger, gas turbine and engine components, rotor blades, pumps and hot working tools.
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 20 - 23 %
20 - 23 %
Cobalt, Co <= 1.0 %
<= 1.0 %
Iron, Fe <= 3.0 %
<= 3.0 %
Molybdenum, Mo 8.0 - 10 %
8.0 - 10 %
Nickel, Ni 61.25 - 68.85 %
61.25 - 68.85 %
Niobium, Nb (Columbium, Cb) 3.15 - 4.15 %
3.15 - 4.15 %
Titanium, Ti <= 0.50 %
<= 0.50 %