Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufTech™ GM-93-060LT PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GM-93-060LT PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: A clear, non-toxic, extrusion compound for food contact use. Compound exhibits excellent low temperature flexibility.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 75.0

@Time 15.0 sec
75.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 17.2 MPa
2490 psi
ASTM D412
Elongation at Break 345 %
345 %
ASTM D412
Processing Properties Metric English Comments
Processing Temperature 160 - 177 °C
320 - 350 °F
Suggested Stock
Users viewing this material also viewed the following: