Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufTech™ GA-509OR-JM PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GA-509OR-JM PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: An 80°C, oil resistant, flexible PVC based compound suitable for jacketing applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 66.0

@Time 15.0 sec
66.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 13.9 MPa
2020 psi
ASTM D412
12.232 MPa

@Temperature 60.0 °C,
Time 605000 sec
1774.1 psi

@Temperature 140 °F,
Time 168 hour
Oil Aged
14.734 MPa

@Temperature 113 °C,
Time 605000 sec
2137.0 psi

@Temperature 235 °F,
Time 168 hour
Oven Aged
Elongation at Break 380 %
380 %
ASTM D412
296.4 %

@Treatment Temp. 60.0 °C,
Time 605000 sec
296.4 %

@Treatment Temp. 140 °F,
Time 168 hour
Oil Aged
349.6 %

@Treatment Temp. 113 °C,
Time 605000 sec
349.6 %

@Treatment Temp. 235 °F,
Time 168 hour
Oven Aged
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Oxygen Index 26.0 %
26.0 %
ASTM D2863
Users viewing this material also viewed the following: