Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL SA120FIN PPE

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL SA120FIN PPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Noryl* SA120FIN resin is a powder version of a low molecular weight polymer based on Polyphenylene ether (PPE). Noryl* SA120FIN is intended for use as additive or building block in a variety of thermoplastics, thermoplastic elastomers like Styrenic Block Copolymers, and thermoset materials like Epoxies, Phenolics, Polyurethanes, and Unsaturated Polyesters. Properties that may be improved by adding Noryl* SA120FIN resin to these thermosets can include: Thermal (glass transition temperature), Adhesion (at elevated temperatures), Mechanical (toughness, dimensional stability), Chemical resistance (acids, bases), Moisture absorption, and Electrical Properties (dielectric constant, dissipation factor).
Physical Properties Metric English Comments
Bulk Density 0.00100 g/cc
0.0000361 lb/in³
ISO 1183
Particle Size <= 63 µm
<= 63 µm
10%; Malvern
<= 125 µm
<= 125 µm
15%; Malvern
<= 425 µm
<= 425 µm
45%; Malvern
<= 710 µm
<= 710 µm
62%; Malvern
<= 1000 µm
<= 1000 µm
100%; Malvern
Viscosity 73400 cP
73400 cP
SABIC Method
Viscosity Measurement 0.12
0.12
Intrinsic Viscosity [dl/g]; SABIC Method
Molecular Weight 6300 g/mol
6300 g/mol
Mw; SABIC Method
Thermal Properties Metric English Comments
Transformation Temperature, Tg 165 °C
329 °F
half width; SABIC Method
Optical Properties Metric English Comments
Gardner Color Number 12
12
20% in Toluene, Initial; SABIC Method
14
14
20% in Toluene, Aged 177C, 24 hrs, nitrogen; SABIC Method
Electrical Properties Metric English Comments
Dielectric Constant 2.54

@Frequency 1.00e+6 Hz
2.54

@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.00070

@Frequency 1.00e+6 Hz
0.00070

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Mn 2350
SABIC Method
Phenolic End-group Content 425µ mol/g
SABIC Method
Physical Form POWDER
SABIC Method
Users viewing this material also viewed the following: