Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX GTX600 PPE+PA6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX GTX600 PPE+PA6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Pa6 based unfilled GTX
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0070 - 0.0090 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
SABIC - Japan Method
Elongation at Break 120 %
120 %
SABIC - Japan Method
Flexural Strength 87.0 MPa
12600 psi
ASTM D790
Flexural Modulus 2.05 GPa
297 ksi
ASTM D790
Izod Impact, Notched 6.37 J/cm
11.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 75.0 - 85.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.7 - 47.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 185 °C

@Thickness 3.20 mm
365 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved