Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp RFZ42 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Thermocomp* RFZ42 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 119 MPa
17300 psi
ASTM D 638
Elongation at Break 2.8 %
2.8 %
ASTM D 638
Tensile Modulus 6.24 GPa
905 ksi
50 mm/min; ASTM D 638
Flexural Strength 179 MPa
26000 psi
ASTM D 790
Flexural Modulus 5.73 GPa
831 ksi
ASTM D 790
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 4.21 J/cm

@Temperature 23.0 °C
7.89 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 241 °C

@Thickness 3.20 mm
466 °F

@Thickness 0.126 in
unannealed; ASTM D 648