Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* MX99432 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 2.9 %
2.9 %
ASTM D638
Tensile Modulus 5.27 GPa
764 ksi
50 mm/min; ASTM D638
Flexural Strength 89.0 MPa
12900 psi
ASTM D790
Flexural Modulus 4.61 GPa
669 ksi
ASTM D790
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.09 J/cm
9.54 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 145 °C

@Thickness 3.20 mm
293 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: