SABIC Innovative Plastics LNP THERMOCOMP 9H0600A

Category Polymer , Thermoplastic
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP 9H0600A.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Thermocomp* 9H0600A is a High Specific Gravity compound containing proprietary fillers.
Physical Properties Metric English Comments
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength at Break 1.00 MPa
145 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 750 %
750 %
Type I, 5 mm/min; ASTM D638