Material Notes:
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for combination printing, process printing, solids and line work. 3M now offers a range of 40 and 60 mil cushioned plate mounting tapes for flexographic printing needs.Information provided by 3M
Physical Properties Metric English Comments
Density 0.562 g/cc
0.0203 lb/in³
Thickness 114 microns
4.50 mil
Film Liner
1070 microns
42.0 mil
Tape
Mechanical Properties Metric English Comments
Compressive Strength 0.138 MPa
20.0 psi
10% Compression, Deflection
0.276 MPa
40.0 psi
25% Compression, Deflection
Peel Strength 0.1643 kN/m
0.9375 pli
Linered side-Photopolymer, Adhesion; ASTM D3330
0.60259 kN/m
3.4375 pli
Non-linered side-Composite Sleeve, Adhesion; ASTM D3330
0.60259 kN/m
3.4375 pli
Non-linered side-Polyester, Adhesion; ASTM D3330
0.60259 kN/m
3.4375 pli
Non-linered side-Urethane-B, Adhesion; ASTM D3330
0.657 kN/m
3.75 pli
Non-linered side-Stainless Steel, Adhesion; ASTM D3330
0.71216 kN/m
4.0625 pli
Non-linered side-Urethane-A, Adhesion; ASTM D3330
Descriptive Properties Value Comments
Liner Firm Blue Foam