Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ICO Polymers ICORENEâ„¢ 150-1496 HDPE Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Rotational Molding Grade
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICORENE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICORENEâ„¢ 150-1496 HDPE Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: ICORENE 150-1496 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is enhanced with ICOPower and RotoGo. The base resin is FDA approved and is fully stabilized to UV8 level. Key Characteristics: high stiffness, high toughness, good processing. Applications: This ICORENE® grade is particularly suitable for use in kayak applications. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D1505
Melt Index of Compound 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 23.309 MPa
3380.7 psi
2"/min; ASTM D638
Elongation at Break 697 %
697 %
2"/min; ASTM D638
Flexural Modulus 0.86798 GPa
125.89 ksi
ASTM D790
Impact 26

@Temperature -40.0 °C
26

@Temperature -40.0 °F
J/mm, instrumented impact, rotomolded test sample; ICO R&D1.14