SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer (Asia Pacific)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 75.0 MPa
10900 psi
ASTM D790
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm
11.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C

@Thickness 3.20 mm
210 °F

@Thickness 0.126 in
unannealed; ASTM D648