Goodfellow Havar® High Permeability Nickel Magnetic Alloy

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Nickel Alloy
Manufacturer Goodfellow
Trade Name Havar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Havar® High Permeability Nickel Magnetic Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A high Nickel, magnetically soft alloy used for magnetic shielding, high quality low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head laminations and magnetometer bobbin cores. Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Component Elements Properties Metric English Comments
Iron, Fe 15 %
15 %
Molybdenum, Mo 5.0 %
5.0 %
Nickel, Ni 80 %
80 %