Solvay MIRASHEEN® CP-820/G Surfactant

Category Fluid
Manufacturer Solvay
Trade Name MIRASHEEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MIRASHEEN® CP-820/G Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: New generation of ready to use, cost effective liquid pearl concentrate. A pumpable liquid that readily blends into formulated shampoos, liquid hand soaps, shower gels and related products to impart opacity and pearlescence.Identification: COCAMIDOPROPYL BETAINE, GLYCOL DISTEARATE, LAURETH-7, SODIUM COCOAMPHOACETATE, SODIUM LAURETH SULPHATE, WATERCAS: 70851-07-9 , 627-83-8 , 68002-97-1 , 68608-65-1 , 91648-56-5, 7732-18-5Available in: Asia Pacific, Europe, Latin America and North America Applications: Usage of MIRASHEEN CP-820/G at 1.0 to 5.0% provides a superior pearlescent effect. The concentrate can be incorporated by mixing it with the base formulation at ambient temperatures followed by pH and viscosity adjustments as required. Slow blending of MIRASHEEN CP-820/G into the formulation with smooth agitation results in a finished product exhibiting excellent pearlescence and stability. MIRASHEEN CP-820/G is also suitable for use over a broad pH range. MIRASHEEN CP-820/G are ready to use liquid pearlising concentrates that deliver excellent pearlescence, as well as distinct emolliency, mildness and moisturising benefits to the skin. In addition, they also contain ingredients that provide viscosity building, foam stability and lather enhancement characteristics. Thanks to the amphoteric and non-ionic components, MIRASHEEN CP series is compatible with all surfactants types. Their unique composition contributes to significant wet-combout. Mild baby-type products and other high foaming Personal Care products may be easily formulated using this cold pearliser, since the ingredients in this concentrate are commonly found in these types of products.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 33 - 38 %

@Temperature 110 °C,
Time 3600 sec
33 - 38 %

@Temperature 230 °F,
Time 1.00 hour
RP-0540
pH 6.0 - 8.0
6.0 - 8.0
10% Aqueous; RP-0420
Brookfield Viscosity <= 10000 cP
<= 10000 cP
#3 sp @ 12 rpm; RP-0596
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Pearlescent flowable paste
RP-0064