Reltek BONDiT™ B-482CC Adhesive and Sealant

Category Polymer , Adhesive
Manufacturer Reltek LLC
Trade Name BONDiT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reltek BONDiT™ B-482CC Adhesive and Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key PropertiesCaulking and sealing dissimilar materials for very harsh environments. Excellent adhesion to most substrates without primer. High impact resistance.ApplicationsCaulks and seals plastics, metals, wood, rubber, urethane, concrete and aggregate. Survives harsh environments, particularly moisture, and very harsh chemical environments, marine and sub sea. Exceptional performance as a universal caulk for industrial applications. Can be applied to oily surfaces. Cures underwater. Ambient 24 hour or accelerated thermal cure.Information provided by Reltek LLC
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
A
1.42 g/cc
1.42 g/cc
B