Quadrant EPP QuickSilver® PE 1000 Truck liners (ISO Data)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Quadrant Engineering Plastics Products
Trade Name Quicksilver®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP QuickSilver® PE 1000 Truck liners (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Medium and heavy duty liners Superior, steady release of materials Abrasion-, corrosion- and chemical-resistant High impact strength Outlasts traditional materials Weighs less than aluminum or steel
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Limited
Limited
Hot Water / Steam Unacceptable
Unacceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Limited
Limited
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable