Formosa Plastics Formolon® AW04 Homopolymer/Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® AW04 Homopolymer/Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Homopolymer/Compound Formolon (AW04) is a NSF approved medium molecular weight dry blend PVC compound. This compound has been engineered primarily for rigid extrusion applications. The exceptional stability properties provide a consistent whiteness that enhances the finish and marketability of the end product. ASTM Classification (for PVC Resin): GP1-1600, ASTM D1755Information provided by Formosa Plastics Corporation, USA
Mechanical Properties Metric English Comments
Tensile Strength 49.6 MPa
7200 psi
ASTM D638
Tensile Modulus 2.83 GPa
410 ksi
Impact 1.1
1.1
[ft-lb/in]; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 169 °C
336 °F
no load specified; ASTM D648