Quadrant EPP Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), 20% Glass Fiber
Manufacturer Quadrant Engineering Plastics Products
Trade Name Duratron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Duratron® U2200 PEI Extruded 20% Glass Reinforced Polyetherimide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc

@Temperature 22.8 °C
1.41 g/cc

@Temperature 73.0 °F
ASTM D792
Water Absorption 0.20 %
0.20 %
IMMERSION; 24HRS.; ASTM D570 2
Water Absorption at Saturation 1.0 %
1.0 %
ASTM D570 2
Mechanical Properties Metric English Comments
Tensile Strength 117 MPa

@Temperature 22.8 °C
17000 psi

@Temperature 73.0 °F
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 179 MPa

@Temperature 22.8 °C
26000 psi

@Temperature 73.0 °F
ASTM D790
Flexural Modulus 4.83 GPa

@Temperature 22.8 °C
700 ksi

@Temperature 73.0 °F
ASTM D790
Compressive Strength 193 MPa

@Strain 10.0 %,
Temperature 22.8 °C
28000 psi

@Strain 10.0 %,
Temperature 73.0 °F
ASTM D695
Compressive Modulus 3.45 GPa

@Temperature 22.8 °C
500 ksi

@Temperature 73.0 °F
ASTM D695
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 210 °C
410 °F
ASTM D3418