Pyrotek TS-83 Thermoset Electrical Insulation Product (Nema Grade: LE)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Pyrotek, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek TS-83 Thermoset Electrical Insulation Product (Nema Grade: LE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Linen reinforcement, Phenolic resin, Tan / Black color. Good electrical and high mechanical strength. Moisture resistant.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
Water Absorption 1.0 %
1.0 %
Mechanical Properties Metric English Comments
Flexural Strength 152 MPa
22000 psi
Compressive Strength 262 MPa
38000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+10 ohm-cm
7.00e+10 ohm-cm
Dielectric Strength 14.0 kV/mm
356 kV/in