Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek PT-10 Graphite

Category Carbon , Graphite
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek PT-10 Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.ApplicationsDegassing shafts Stators Pump shafts and posts AdvantagesHigh strength Up to 2-3 times the life, depending on the application Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
Porosity 6.0 %
6.0 %
Mechanical Properties Metric English Comments
Flexural Strength 26.0 MPa
3770 psi
across grain
28.0 MPa
4060 psi
with grain
Compressive Strength 41.0 MPa
5950 psi
across grain
48.0 MPa
6960 psi
with grain
Thermal Properties Metric English Comments
CTE, linear 3.40 µm/m-°C

@Temperature 20.0 °C
1.89 µin/in-°F

@Temperature 68.0 °F
with grain
4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
across grain
Users viewing this material also viewed the following: