Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymax® Maxelast® S4845 TPE, PS Overmold

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Nagtong Polymax
Trade Name Maxelast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymax® Maxelast® S4845 TPE, PS Overmold.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 45

@Time 10.0 sec
45

@Time 0.00278 hour
ASTM D2240
Tensile Stress 2.01 MPa

@Strain 100 %
292 psi

@Strain 100 %
ASTM D412
3.24 MPa

@Strain 300 %
470 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield 4.89 MPa
709 psi
ASTM D412
Elongation at Break 710 %
710 %
ASTM D412