| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Stress |
3.24
MPa @Strain 300 % |
470
psi @Strain 300 % |
ASTM D412 |
|
Polymax® Maxelast® A9860 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
|
|||
| Tensile Stress |
3.24
MPa @Strain 300 %, Temperature 23.0 °C |
470
psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
|
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce..
|
|||
| Tensile Stress |
3.24
MPa @Strain 300 %, Temperature 23.0 °C |
470
psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
|
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro..
|
|||
| Tensile Stress |
3.24
MPa @Strain 300 % |
470
psi @Strain 300 % |
ASTM D412 |
|
Polymax® Maxelast® S4845 TPE, PS Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong ..
|
|||
| Tensile Stress |
3.24
MPa @Strain 300 %, Temperature 23.0 °C |
470
psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
|
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
|
|||
| Tensile Stress |
3.24
MPa @Strain 20.06 %, Temperature 100 °C |
470
psi @Strain 20.06 %, Temperature 212 °F |
ISO 527 |
|
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
|
|||
| Tensile Stress |
3.24
MPa @Strain 14.34 %, Temperature 120 °C |
470
psi @Strain 14.34 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
|
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
|
|||