Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synplast™ 9P-N Di Nonyl Phthalate

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer PolyOne Corporation
Trade Name Synplast™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synplast™ 9P-N Di Nonyl Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Linear phthalate esterInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.962 - 0.968 g/cc

@Temperature 25.0 °C
0.962 - 0.968 g/cc

@Temperature 77.0 °F
ASTM D4052
Kinematic Viscosity 46 cSt

@Temperature 25.0 °C
46 cSt

@Temperature 77.0 °F
ASTM D445
Molecular Weight 420 g/mol
420 g/mol
Theoretical
Vapor Pressure 0.00133 bar

@Temperature 200 °C
0.998 torr

@Temperature 392 °F
ASTM Color 25
25
Pt-Co Scale, Maximum; ASTM D1209
Thermal Properties Metric English Comments
Pour Point -50.0 °C
-58.0 °F
Optical Properties Metric English Comments
Refractive Index 1.48

@Temperature 25.0 °C
1.48

@Temperature 77.0 °F
Chemical Properties Metric English Comments
Total Acid Number <= 0.10
<= 0.10
[mg KOH/g]; ASTM D1045
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
ASTM D1533
Descriptive Properties Value Comments
Appearance Clear, clean
ASTM D2090
Clear/Transparent
Ester Content 99%
ASTM D3465; Minimum
Forms Liquid
Generic Material Di Nonyl Phthalate
Generic Name Di Nonyl Phthalate
Processing Method Calendering
Compounding
Plastisol
Regional Availability Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Interior Parts
Cable Jacketing
Film
Sheet
Wire & Cable Applications
Users viewing this material also viewed the following: