Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding

Category Polymer , Thermoplastic , Liquid Crystal Polymer (LCP) , Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne™ Corporation
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Linear Mold Shrinkage 0.00010 cm/cm
0.00010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 117 MPa
17000 psi
ASTM D638
Elongation at Break 0.50 %
0.50 %
ASTM D638
Tensile Modulus 34.5 GPa
5000 ksi
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 27.6 GPa
4000 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
ASTM D257
Surface Resistivity per Square <= 1.00e+7 ohm
<= 1.00e+7 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 316 - 343 °C
600 - 650 °F
Mold Temperature 135 - 149 °C
275 - 300 °F
Drying Temperature 135 - 149 °C
275 - 300 °F
Users viewing this material also viewed the following: