Physical Properties Metric English Comments
Melt Flow 1.4 g/10 min
1.4 g/10 min
Cond. Q; ASTM D1238
Multibase Nylex™ 2185 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Multibase Nylex™ 2185 Polyamide + PP
Forms: PelletsInformation provided by Multibase
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
PolyOne Maxxam™ FR PP H6 GF25 NHFR grey Polypropylene, Unspecified (PP, Unspecified)
Information provided by PolyOne
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene
Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte..
Melt Flow 1.4 - 2.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 - 2.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
NIZHNEKAMSKNEFTEKHIM PP 1500H (S30G) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
Melt Flow 1.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM Data
Americas Styrenics Styron® 613 Polystyrene  (discontinued **)
STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer.
Melt Flow 1.4 g/10 min
1.4 g/10 min
ASTM D1238
Hyosung Topilene B301 PP
B301 HomopolymerApplications:Thermoforming sheetsCharacteristics:High melt tensionDimensional stabilityGood optical propertyInformation provided by Hyosung Corporation
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate
Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h..
Melt Flow 1.4 g/10 min

@Load 6.60 kg,
Temperature 295 °C
1.4 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 9076 PEI
Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Melt Flow 1.4 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.4 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Silon Tabond 2002 Adhesive Resin
TABOND 2002 is ethylene-octene Plastomer / LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Silon Tabond 2004 Adhesive Resin
TABOND 2004 is a copolymer modified with maleic anhydride functional groups.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon, EVOH, PET, PBT, PC, aluminium, copper, brass ..
Melt Flow 1.4 g/10 min
1.4 g/10 min
ASTM D1238
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio..
Melt Flow 1.4 g/10 min

@Load 21.6 kg,
Temperature 190 °C
1.4 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133/G
Total HDPE 56020 S XP High Density Polyethylene - Blow Molding
HDPE 56020 S XP is a very high molecular weight (VHMW) high density polyethylene with a high resistance to impact, good chemical resistance and optimized balance between Environmental Stress Crack R..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips MarFlex® D143FK Metallocene Linear Low Density Polyethylene, Blown Film
This mLLDPE is tailored for applications that require:Excellent clarityExcellent glossExcellent toughnessExcellent heat sealTypical blown film applications include:Seal layer in coextrusionsHeavy du..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont™ Fusabond® C250 Polymer Modifier
DuPont™ Fusabond® C250 is a modified ethylene vinyl acetate copolymer. Used as an adhesion promoter and coupling agent.
Melt Flow 1.4 g/10 min
1.4 g/10 min
ASTM D1238
Aclo Accutech ABS ABS833G10L Glass Reinforced
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem LD5000A LDPE Blow Molding Polyethylene
LD5000A is a low-density polyethylene with good mechanical properties, good ESCR, and excellent sealing characteristics. It does not contain additives. It is used in general purpose blow molded arti..
Melt Flow 1.4 g/10 min
1.4 g/10 min
Ashley Polymers Ashlene® ABS Resin 223
Medium impact, medium flow, matte finish. Suitable for general purpose injection molding.Data provided by the manufacturer
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Phillips 66 COPYLENE® CH014 Polypropylene, Homopolymer, Extrusion, Strapping
COPYLENE™ CH014 is a polypropylene homopolymer resin designed for extrusion applications. Applications: Raffia/Tapes/Strapping; Geotextile & Agriculture; Nets. Equivalent to Pro-fax® HL781GInforma..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati..
Melt Flow 1.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
Chevron Phillips EA3025 Crystal Polystyrene  (discontinued **)
High heat crystal polystyrene.Applications:Foam egg cartonsFoam meat traysInsulation boardBi-axially oriented sheetFeatures:Ultra-high molecular weight homopolymerHigh Vicat softening temperatureNar..
Melt Flow 1.4 g/10 min

@Load 6.60 kg,
Temperature 295 °C
1.4 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 9076 PEI (Asia Pacific)
Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate
Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym..
Melt Flow 1.4 - 1.7 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.4 - 1.7 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Granulate; ISO 1133/H
SYNTHOS Krasten® 171 General Purpose Polystyrene
Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high ..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer.
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer
Key Features: fast crystallization shortens cycle times, excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive blow molded partsMeets FDA requir..