Material Notes:
Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 3.45 GPa
500 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 37.9 MPa
5500 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256