| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable 1604-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 87 | 87 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 20.3 MPa | 2940 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 260 % | 260 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
| 75.0 °C | 167 °F | UL Temperature Rating | |
| Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
| Oxygen Index | 32 % @Thickness 1.91 mm |
32 % @Thickness 0.0752 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 174 - 182 °C | 345 - 360 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Lead Stabilizer | |
| Agency Ratings | NEC Article 725 | |
| NEC Article 760 | ||
| NEC Article 800 | ||
| Features | Flame Retardant | |
| General Purpose | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion Coating | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Retention of Tensile Elongation | 88% | 113°C, 1.91 mm; 168 hr, UL Standard |
| Retention of Tensile Strength | 98% | 113°C, 1.91 mm; 168 hr, UL Standard |
| Uses | Cable Jacketing | |
| Communication Wire Jacketing | ||
| Wire & Cable Applications | ||
| Wire Types | CL2 | |
| CL2R | ||
| CL3R | ||
| CMR | ||
| FPLR |