| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible XV3683 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | ASTM D792 |
| Volatiles | 0.20 % @Thickness 1.91 mm, Temperature 105 °C |
0.20 % @Thickness 0.0752 in, Temperature 221 °F |
Loss; Method A; ASTM D1203B |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 77 | 77 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 12.3 MPa | 1780 psi | Type IV, 510 mm/min; ASTM D638 |
| Tensile Strength | 6.55 MPa @Strain 100 % |
950 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 400 % | 400 % | Type IV, 510 mm/min; ASTM D638 |
| Tear Strength | 109 kN/m | 622 pli | Die C, 510 mm/min; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -33.9 °C | -29.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 177 - 182 °C | 351 - 360 °F | |
| 193 - 199 °C | 379 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Good Abrasion Resistance | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Profile Extrusion | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Gaskets | |
| Hose | ||
| Profiles | ||
| Seals | ||
| Tubing |