| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible R3090S Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 66 | 66 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 11.0 MPa | 1600 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 370 % | 370 % | Type IV, 510 mm/min; ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -34.0 °C | -29.2 °F | ASTM D746 |
| Flammability, UL94 | V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
BK; Internal Method |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
NC; Internal Method | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
RD; Internal Method | |
| Oxygen Index | 21 % @Thickness 1.91 mm |
21 % @Thickness 0.0752 in |
ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 155 - 165 °C | 311 - 329 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Agency Ratings | UL QMFZ2 | |
| Appearance | Clear/Transparent | |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion Coating | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Retention of Tensile Elongation | 80% | 136°C, 1.91 mm; 168 hr, UL Standard |
| Retention of Tensile Strength | 110% | 136°C, 1.91 mm; 168 hr, UL Standard |
| RoHS Compliance | RoHS Compliant | |
| Uses | Cable Jacketing | |
| Flexible Cord Jacketing | ||
| Wire & Cable Applications |