| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible 90401 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.24 g/cc | 1.24 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 75 | 75 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 14.2 MPa | 2060 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 310 % | 310 % | Type IV, 510 mm/min; ASTM D638 |
| Tear Strength | 36.0 kN/m | 205 pli | Die C, 510 mm/min; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flame Spread | 0.00 mm/min | 0.00 in/min | Automotive Burn Test; FMVSS 302 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Gloss | 4.0 % | 4.0 % | 60°; ASTM D523 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive Specifications | GM GMP.PVC.077 | |
| Cold Flexibility | Pass | GM 9503P; -29°C, 1.91 mm; 25 mm, 4 hr |
| Features | Low Gloss | |
| Fogging | 86% | SAE J1756; 3 hrs, 212°F(100°C), 70°F(21°C), after 1 hour |
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Blow Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Automotive Applications | |
| Automotive Interior Trim | ||
| Xenon Weatherometer | Pass | SAE J1960; Interior, 1240 kJ/m², All Colors, dE*<3.0 |