| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Geon™ Vinyl Flexible 90059 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Volatiles | 0.45 % <br>@Thickness 1.91 mm,<br> Temperature 105 °C |
0.45 % <br>@Thickness 0.0752 in,<br> Temperature 221 °F |
Loss; Method A; ASTM D1203B |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 37 | 37 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 23.6 MPa | 3420 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 290 % | 290 % | Type IV, 510 mm/min; ASTM D638 |
| Tear Strength | 75.0 kN/m | 428 pli | Die C, 2 in/min; ASTM D1004 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive Specifications | GM GMP.PVC.003 | |
| Features | Low Gloss | |
| Forms | Pellets | |
| Fungal Resistance | Pass | ASTM G21 |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Low Temperature Flexibility | Pass | -30°C, 1.91 mm; 4 hr, 25 mm |
| Processing Method | Extrusion | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Automotive Applications | |
| Beltline Moldings | ||
| Outdoor Applications | ||
| Xenon Weatherometer | Pass | SAE J1960; Exterior, 2000 kJ/m², Natural, dE*<3.0 |