| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible 90055 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
| Volatiles | 0.34 % @Thickness 1.91 mm, Temperature 105 °C |
0.34 % @Thickness 0.0752 in, Temperature 221 °F |
Loss; Method A; ASTM D1203B |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 83 | 83 | 15 sec; ASTM D2240 |
| Tensile Strength at Break | 17.4 MPa | 2520 psi | Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 310 % | 310 % | Type IV, 510 mm/min; ASTM D638 |
| Tear Strength | 55.0 kN/m | 314 pli | Die C, 2 in/min; ASTM D1004 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flame Spread | 14 mm/min | 0.55 in/min | Automotive Burn Test; FMVSS 302 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Automotive Specifications | CHRYSLER MS-DC211 Type B CPN3912 Color: 100% Color Match | |
| FORD WSK-M4D689-A2 | ||
| GM GMP.PVC.010 | ||
| Features | High Gloss | |
| Forms | Pellets | |
| Fungal Resistance | Pass | ASTM G21 |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Low Temperature Flexibility | Pass | -29°C, 508.0 µm; 4 hr, 12 mm |
| Processing Method | Extrusion | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Automotive Applications | |
| Automotive Exterior Trim | ||
| Beltline Moldings | ||
| Outdoor Applications | ||
| Xenon Weatherometer | Pass | SAE J1960; Exterior, 2500 kJ/m², All Colors, dE*<3.0 |