Poco Graphite SUPERSiC® Basic Silicon Carbide

Category Ceramic , Carbide
Manufacturer Poco Graphite
Trade Name SUPERSiC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite SUPERSiC® Basic Silicon Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for specific applications.POCO’s unique conversion process produces the highest quality silicon carbide products available on the market today. This process starts with graphite material specially designed and manufactured for use as the precursor in the conversion process. Near net parts are machined in graphite, purified, and subjected to a proprietary conversion process which substitutes pure silicon atoms for carbon atoms. The result is SUPERSIC, POCO’s high purity silicon carbide.
Physical Properties Metric English Comments
Bulk Density 2.53 g/cc
0.0914 lb/in³
Apparent Bulk Density 3.13 g/cc
0.113 lb/in³
Open Porosity 19 %
19 %
Porosity 20 %
20 %
Mechanical Properties Metric English Comments
Hardness, Knoop 1992
1992
[kg/mm<sup>2</sup>]
Tensile Strength, Yield 129 MPa
18700 psi
Modulus of Elasticity 216 GPa
31300 ksi
Flexural Strength 155 MPa
22500 psi
Compressive Strength 110 MPa
16000 psi
Poissons Ratio 0.17
0.17
Fracture Toughness 2.30 MPa-m½
2.09 ksi-in½
Shear Modulus 96.0 GPa
13900 ksi
Dynamic
Thermal Properties Metric English Comments
CTE, linear 2.40 µm/m-°C
1.33 µin/in-°F
at RT
Thermal Conductivity 170 W/m-K
1180 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.400 ohm-cm
0.400 ohm-cm
Descriptive Properties Value Comments
Specific stiffness 85 5N.m/g
Total Impurity Level (ppm), Max 10