Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SSH hardness is 67.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small particle size allow fabrication of complex components containing tight tolerances. Post synthesis treatments available include purification or impregnation with resins, oxidation inhibitors, or metals. Surface treatments offer improved wear characteristics and particle reduction.Some applications of Poco specialty graphites include anode plates for wet cells, fuel cell plates for solid polymer cells, air bearings, hot gas valves, high temperature bearings, bushings, and seals, hot press dies and rams, furnace furniture/fixturing, rocket engine nozzles, molten metal casting components, vacuum furnace heating elements, space vehicle nose cones, mirrors and optical structures, and satellite heat shields.Information provided by Poco Graphite, Inc.
Physical Properties Metric English Comments
Apparent Bulk Density 3.12 g/cc
0.113 lb/in³
Particle Size 5.0 µm
5.0 µm
Mechanical Properties Metric English Comments
Flexural Strength 115 MPa
16700 psi
Compressive Yield Strength 210 MPa
30500 psi
Thermal Properties Metric English Comments
CTE, linear 8.70 µm/m-°C

@Temperature 20.0 °C
4.83 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 175 W/m-K
1210 BTU-in/hr-ft²-°F
Estimated by Poco
Maximum Service Temperature, Air 500 °C
932 °F
Oxidation threshold
Electrical Properties Metric English Comments
Electrical Resistivity 0.000250 ohm-cm
0.000250 ohm-cm