Nabaltec NABALOX® NO 105-71 RA Calcined Aluminum Oxide

Category Ceramic , Oxide , Aluminum Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Nabaltec GmbH
Trade Name NABALOX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec NABALOX® NO 105-71 RA Calcined Aluminum Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insulationhigh mechanical strengthhigh temperature propertiesdimensional accuracyoptimized chemical resistanceChemical industry, Glass industry, Corundum, Refractory industry, Household ceramics, Electroceramics, Engineering ceramicsInformation provided by Nabaltec.
Physical Properties Metric English Comments
Bulk Density 0.950 g/cc
0.0343 lb/in³
Density 3.90 g/cc
0.141 lb/in³
Grain Size 80 µm
80 µm
Median
Particle Size <= 45 µm
<= 45 µm
0.2
Specific Surface Area 0.50 m²/g
0.50 m²/g
BET
Component Elements Properties Metric English Comments
Al2O3 99.8 %
99.8 %
Fe2O3 0.030 %
0.030 %
Na2O 0.10 %
0.10 %
SiO2 0.020 %
0.020 %
Descriptive Properties Value Comments
a-Al2O3 Content % 98
Angle of Response ° 40