Material Notes:
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency.Features: Excellent balance of stiffness and impact strengthExcellent long term heat aging propertiesExcellent color and processing stabilitySuperior weld-line strengthApplications: Woven productsCarpet backing, sacking, industrial and geotextile fabricsCertifications: Pinnacle's polypropylene, as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form complies with appropriate requirements of CFR Title 21, Part 177, Subpart B, Section 177.1520 (c) 1.1a entitled “Olefin Polymers” of the Food Additives Amendment of 1958 to the United States Food, Drug and Cosmetic Act of 1938. Specific limitations or conditions of use apply.Information provided by Pinnacle Polymers.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
Condition L 230/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa

@Thickness 3.20 mm
3300 psi

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Elongation at Yield 7.0 %

@Thickness 3.20 mm
7.0 %

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Flexural Modulus 1.10 GPa

@Thickness 3.20 mm
160 ksi

@Thickness 0.126 in
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A
Izod Impact, Notched 1.07 J/cm

@Thickness 3.20 mm,
Temperature 22.8 °C
2.00 ft-lb/in

@Thickness 0.126 in,
Temperature 73.0 °F
injection molded ASTM Type 1 specimen; ASTM D256
Gardner Impact 21.5 J

@Temperature -30.0 °C
15.8 ft-lb

@Temperature -22.0 °F
Method G, geometry GC; ASTM D5420