Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SHIELD® 2054 Conductive Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 2054 Conductive Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used for electronic enclosures.Application: With their excellent leveling and uniformity, these coatings are compatible with all commercially available application technologies, including high volume/low pressure (HVLP) spray systems, and conventional propeller-agitated pressure pots. As low-settling compounds, they are ready for use after simple mixing in a paint shaker. They are supplied ready-to-spray, and don’t required additional thinning, although MEK can be used.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.60 g/cc
1.20 - 1.60 g/cc
Volatile Organic Compounds (VOC) Content 75 g/l
75 g/l
Brookfield Viscosity 1200 - 1600 cP
1200 - 1600 cP
100 rpm. spindle #3 @ 25°C; Suggested Spraying Viscosity #2 Zahn Cup
Thickness 38.0 microns
1.50 mil
Recommended
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.030 ohm

@Thickness 0.0381 mm
<= 0.030 ohm

@Thickness 0.00150 in
Shielding Effectiveness 75 dB
75 dB
minus water
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 24.0 °C
0.250 hour

@Temperature 75.2 °F
followed by 30 min @ 65°-85°C
1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Consistency Thin Fluid
Coverage 10.4 m2/liter
0.025 mm thick
Filler Silver plated Copper
Mix 1-part
Polymer Water-based acrylic/urethane
Users viewing this material also viewed the following: