| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Peel Strength | 1.58 kN/m | 9.00 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after solder float; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Adhesion Strength, Tape Property; Arlon SQA-TMS-047 |
| Arlon A4020-C004FR 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 15% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film FAR 25.853 Recognition: Product is des.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength; Arlon SQA-TMS-011 |
| Arlon 28751R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | After Thermal Stress; IPC TM-650 2.4.8 |
| Arlon 49N Multifunctional Epoxy Low-Flow Prepreg 49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength; ASTM D624 |
| Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength (S1 to S1); ASTM D624 |
| Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength (S1 to S1); ASTM D624 |
| Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength (S1 to S1); ASTM D624 |
| Arlon 55986R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | To Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2 |
| Arlon CLTE-AT Commercial Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength (S1 to S1); Arlon SQA-TMS-011 |
| Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength; Arlon SQA-TMS-011 |
| Arlon R35551X015 0.015" Uncured Silicone Rubber with Woven Fabric Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Primed 3M Nextel 312 Woven Fabric AF-10, HCSide 2: Uncured Silicone RubberThis data represents typica.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength (S1 to S1); ASTM D624 |
| Arlon R36029R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass This data represents typical values for the production .. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | 180°, Polystyrene |
| 3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | Bond Strength; Arlon SQA-TMS-011 |
| Arlon 51946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat Appearance: Brown silicone rubber and gum on fiberglass.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | on canvas |
| 3M Scotch-Weld™ 3776LM Low Melt Adhesive Bonds variety of plastics, woods and light-gauge metals and use with low melt applicator onlyInformation provided by 3M |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | 180° T-Peel, Black SBR/CRS |
| 3M Scotch-Weld™ DP820 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP820 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | to Stainless Steel; ASTM D3330 |
| 3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after solder float; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after solder float; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after exposure to process solutions; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | after solder float; IPC-TM-650.2.4.8 |
| Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
| Peel Strength | 1.58 kN/m | 9.00 pli | After Thermal Stress; IPC TM-650 2.4.8 |
| Arlon 47N Quick Cure Epoxy Low-Flow Prepreg 47N is a low-flow epoxy prepreg engineered for binding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. An optional low lamination temperature protects components already mou.. |
|||