| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.611 g/cc @Temperature 232 °C |
0.0221 lb/in³ @Temperature 450 °F |
|
| 0.647 g/cc @Temperature 177 °C |
0.0234 lb/in³ @Temperature 350 °F |
||
| 0.695 g/cc @Temperature 121 °C |
0.0251 lb/in³ @Temperature 250 °F |
||
| 0.731 g/cc @Temperature 65.6 °C |
0.0264 lb/in³ @Temperature 150 °F |
||
| 0.755 g/cc @Temperature 23.9 °C |
0.0273 lb/in³ @Temperature 75.0 °F |
||
| 0.767 g/cc @Temperature 15.6 °C |
0.0277 lb/in³ @Temperature 60.0 °F |
||
| 0.791 g/cc @Temperature -17.8 °C |
0.0286 lb/in³ @Temperature 0.000 °F |
||
| 0.815 g/cc @Temperature -45.6 °C |
0.0294 lb/in³ @Temperature -50.0 °F |
||
| 0.827 g/cc @Temperature -73.3 °C |
0.0299 lb/in³ @Temperature -100 °F |
||
| Viscosity | 0.18 cP @Temperature 232 °C |
0.18 cP @Temperature 450 °F |
|
| 0.26 cP @Temperature 177 °C |
0.26 cP @Temperature 350 °F |
||
| 0.42 cP @Temperature 121 °C |
0.42 cP @Temperature 250 °F |
||
| 0.80 cP @Temperature 65.6 °C |
0.80 cP @Temperature 150 °F |
||
| 1.5 cP @Temperature 23.9 °C |
1.5 cP @Temperature 75.0 °F |
||
| 5.0 cP @Temperature -17.8 °C |
5.0 cP @Temperature 0.000 °F |
||
| 16 cP @Temperature -45.6 °C |
16 cP @Temperature -50.0 °F |
||
| 154 cP @Temperature -73.3 °C |
154 cP @Temperature -100 °F |
||
| Viscosity Measure | 0.30 cSt @Temperature 232 °C |
0.30 cSt @Temperature 450 °F |
|
| 0.40 cSt @Temperature 177 °C |
0.40 cSt @Temperature 350 °F |
||
| 0.61 cSt @Temperature 121 °C |
0.61 cSt @Temperature 250 °F |
||
| 1.0 cSt @Temperature 65.6 °C |
1.0 cSt @Temperature 150 °F |
||
| 2.0 cSt @Temperature 23.9 °C |
2.0 cSt @Temperature 75.0 °F |
||
| 5.9 cSt @Temperature -17.8 °C |
5.9 cSt @Temperature 0.000 °F |
||
| 19 cSt @Temperature -45.6 °C |
19 cSt @Temperature -50.0 °F |
||
| 185 cSt @Temperature -73.3 °C |
185 cSt @Temperature -100 °F |
||
| Molecular Weight | 160 g/mol | 160 g/mol | average |
| Vapor Pressure | 0.0400 bar @Temperature 107 °C |
30.0 torr @Temperature 225 °F |
|
| 0.0667 bar @Temperature 121 °C |
50.0 torr @Temperature 250 °F |
||
| 0.108 bar @Temperature 135 °C |
81.0 torr @Temperature 275 °F |
||
| 0.193 bar @Temperature 149 °C |
145 torr @Temperature 300 °F |
||
| 0.500 bar @Temperature 177 °C |
375 torr @Temperature 350 °F |
||
| 1.04 bar @Temperature 204 °C |
780 torr @Temperature 400 °F |
||
| 1.25 bar @Temperature 218 °C |
938 torr @Temperature 425 °F |
||
| 1.421 bar @Temperature 232 °C |
1066 torr @Temperature 450 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Vaporization | 262 J/g | 113 BTU/lb | |
| Specific Heat Capacity | 1.63 J/g-°C @Temperature -73.3 °C |
0.390 BTU/lb-°F @Temperature -100 °F |
|
| 1.76 J/g-°C @Temperature -45.6 °C |
0.420 BTU/lb-°F @Temperature -50.0 °F |
||
| 1.84 J/g-°C @Temperature -17.8 °C |
0.440 BTU/lb-°F @Temperature 0.000 °F |
||
| 2.01 J/g-°C @Temperature 23.9 °C |
0.480 BTU/lb-°F @Temperature 75.0 °F |
||
| 2.18 J/g-°C @Temperature 65.6 °C |
0.520 BTU/lb-°F @Temperature 150 °F |
||
| 2.38 J/g-°C @Temperature 121 °C |
0.570 BTU/lb-°F @Temperature 250 °F |
||
| 2.59 J/g-°C @Temperature 177 °C |
0.620 BTU/lb-°F @Temperature 350 °F |
||
| 2.80 J/g-°C @Temperature 232 °C |
0.670 BTU/lb-°F @Temperature 450 °F |
||
| Thermal Conductivity | 0.131 W/m-K @Temperature 232 °C |
0.912 BTU-in/hr-ft²-°F @Temperature 450 °F |
|
| 0.137 W/m-K @Temperature 177 °C |
0.948 BTU-in/hr-ft²-°F @Temperature 350 °F |
||
| 0.142 W/m-K @Temperature 121 °C |
0.984 BTU-in/hr-ft²-°F @Temperature 250 °F |
||
| 0.147 W/m-K @Temperature 65.6 °C |
1.02 BTU-in/hr-ft²-°F @Temperature 150 °F |
||
| 0.1504 W/m-K @Temperature 23.9 °C |
1.044 BTU-in/hr-ft²-°F @Temperature 75.0 °F |
||
| 0.1539 W/m-K @Temperature -17.8 °C |
1.068 BTU-in/hr-ft²-°F @Temperature 0.000 °F |
||
| 0.1574 W/m-K @Temperature -45.6 °C |
1.092 BTU-in/hr-ft²-°F @Temperature -50.0 °F |
||
| 0.1591 W/m-K @Temperature -73.3 °C |
1.104 BTU-in/hr-ft²-°F @Temperature -100 °F |
||
| Boiling Point | 202 °C | 396 °F | |
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| 260 °C | 500 °F | max. recommended film temperature | |
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
| Flash Point | >= 54.4 °C | >= 130 °F | closed cup; ASTM D56 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.84e+14 ohm-cm | 1.84e+14 ohm-cm | |
| Dielectric Constant | 2.03 @Frequency 1000 Hz |
2.03 @Frequency 1000 Hz |
ASTM D924-04 |
| Dielectric Breakdown | 22150 V @Thickness 2.54 mm |
22150 V @Thickness 0.100 in |
ASTM D1816-04 |
| Dissipation Factor | 0.000010 @Frequency 1000 Hz |
0.000010 @Frequency 1000 Hz |
ASTM D924-04 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | water white | |
| Autoignition | >500°F | < 10 sec delay |
| Feedstock | hydrocarbon | |
| Odor | none |