Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers SOFTAPLAS™ S 65A Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Ovation Polymers
Trade Name SOFTAPLAS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers SOFTAPLAS™ S 65A Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic Elastomer – Excellent hydrolytic Stability and balance of properties. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Melt Index of Compound 6.0 g/10 min

@Load 3.80 kg,
Temperature 190 °C
6.0 g/10 min

@Load 8.38 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 65
63 - 65
15 sec; ASTM D2240
Elongation at Break >= 600 %
>= 600 %
50 mm/min; ASTM D638
Izod Impact, Notched NB
NB
ASTM D256