Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Nemcon™ E - PP AS Polypropylene, Anti-Static

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ E - PP AS Polypropylene, Anti-Static.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nemcon™ E-Series products are designed for use in ESDA electronic assembly environments. E PP AS is a moisture independent anti-static polypropylene characterized by consistent moldability and recyclability.All properties after 48hrs conditioning at 23°C/50% RH
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
50 mm/min; ASTM D638
Elongation at Break 170 %
170 %
50 mm/min; ASTM D638
Tensile Modulus 0.740 GPa
107 ksi
50 mm/min; ASTM D638
Flexural Strength 24.0 MPa
3480 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 0.525 GPa
76.1 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.934 J/cm
1.75 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+10 - 3.00e+11 ohm
1.00e+10 - 3.00e+11 ohm
ASTM D257