Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Osprey Metals 17-4 PH Stainless Steel Powder (Grade 80% - 22)

Category Metal , Ferrous Metal , Stainless Steel , Precipitation Hardening Stainless
Manufacturer Osprey Metals, Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Osprey Metals 17-4 PH Stainless Steel Powder (Grade 80% - 22).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Particle size distribution 1-250 microns. Typical distribution:80% < 22 microns67% < 16 microns43% < 10 microns14% < 5 micronsMean size is 12 microns.Material Notes: Composition above is typical of 17-4 PH precipitation hardening stainless. This alloy is widely used because of its high strength, high hardness, excellent corrosion resistance, and easy heat treatment. The 17-4 PH alloy is used in aerospace, medical, food processing, and chemical industries for applications such as pump shafts, valve stems, braces, fasteners, coupling, rocket and missile components, hydraulic actuators, and wear rings. SHAPE: Predominantly spherical PACKAGING: 4 & 20 Kg. Chemical composition and particle size distribution can be adjusted to suit customers' requirements.The specifications listed are subject to the benefits and scrutiny of Osprey's accreditation to ISO 9001. If the product delivered does not substantially meet the specification, Osprey will replace it. Osprey's liability is limited to the cost of replacement. Information provided to MatWeb by Osprey Metals.
Physical Properties Metric English Comments
Particle Size 12 µm
12 µm
Mean
Component Elements Properties Metric English Comments
Carbon, C 0.010 - 0.070 %
0.010 - 0.070 %
Chromium, Cr 15.5 - 17.5 %
15.5 - 17.5 %
Copper, Cu 3.0 - 5.0 %
3.0 - 5.0 %
Iron, Fe 71.85 %
71.85 %
Manganese, Mn 0.76 %
0.76 %
Typical
<= 1.0 %
<= 1.0 %
Molybdenum, Mo <= 0.30 %
<= 0.30 %
Nickel, Ni 3.0 - 5.0 %
3.0 - 5.0 %
Niobium, Nb (Columbium, Cb) 0.15 - 0.45 %
0.15 - 0.45 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si 0.84 %
0.84 %
Typical
<= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %