Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Omni Plastics OmniTuff™ HPP GRC20 Homopolymer Polypropylene Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Omni Plastics
Trade Name OmniTuff™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Omni Plastics OmniTuff™ HPP GRC20 Homopolymer Polypropylene Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni Plastics
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Flexural Modulus 4.41 GPa
640 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
ASTM D256