Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Okulen® 1000 PE-UHMW, Green Black

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Okulen
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Okulen® 1000 PE-UHMW, Green Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal for applications like machine construction, plant construction, and conveyor technology.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183-A
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength, Yield 14.0 - 17.0 MPa
2030 - 2470 psi
50 mm/min; ISO/R 527
Elongation at Break >= 50 %
>= 50 %
50 mm/min; ISO/R 527
Creep Strength 10.0 MPa
1450 psi
Coefficient of Friction, Dynamic 0.15

@Pressure 2.00 MPa
0.15

@Pressure 290 psi
PE-metal, V = 10 m/min; ASTM D1894
Coefficient of Friction, Static 0.20

@Pressure 2.00 MPa
0.20

@Pressure 290 psi
PE-metal, V = 10 m/min; ASTM D1894
Abrasion 140
140
Slurry-Test rel to GUR 4120 = 100%; DIN 58836
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C
111 µin/in-°F
DIN 53752
Melting Point 135 - 137 °C
275 - 279 °F
DSC ISO 3146
Maximum Service Temperature, Air 80.0 °C
176 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+14 ohm-cm
<= 1.00e+14 ohm-cm
Teil 30; IEC 600093 / VDE 0303
Descriptive Properties Value Comments
FDA Approved No
Users viewing this material also viewed the following: