Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oceanchem Group Antioxidant 1076

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Oceanchem Group Antioxidant 1076.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Molecular Formula: C35H62O3Cas No.: 2082-79-3Property: This product is a nonpolluting nontoxic antioxidant with good heat-resisting and water-extracting performance.Characteristics and Uses: This product is a nonpolluting nontoxic antioxidant with good heat-resisting and water-extracting performance. Wnameely applied to polyolefin, polyamnamee, polyester, polyvinyl chlornamee, ABS resin and petroleum product, often used with DLTP for promoting the antioxnameative effect.Storing, Transporting and Packing: This product is stable without special demands for storing, but high temperature and moisture should be avonameed. Packed in cardboard pails lined with plastic bags with the capacity of 25 kg.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Molecular Weight 530.87 g/mol
530.87 g/mol
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 49.0 - 54.0 °C
120 - 129 °F
Optical Properties Metric English Comments
Transmission, Visible >= 96 %
<br>@Wavelength 425 nm
>= 96 %
<br>@Wavelength 425 nm
10g/100ml Toluene
>= 98 %
<br>@Wavelength 500 nm
>= 98 %
<br>@Wavelength 500 nm
10g/100ml Toluene
Descriptive Properties Value Comments
Appearance White, tasteless crystalline powder
CAS Number 2082-79-3
Chemical Name B -(3,5-tertiary butyl-4-hydroxyl phenyl) propionic18-Calkyl
Content (%) >98.0
Molecular Formula C<sub>35</sub>H<sub>62</sub>O<sub>3</sub>