| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity Measurement | 345 | 345 | Viscosity Index of Base Oil; ASTM D2270 |
| Kinematic Viscosity at 40°C (104°F) | 140 cSt | 140 cSt | Base Oil; ASTM D445 |
| Kinematic Viscosity at 100°C (212°F) | 45 cSt | 45 cSt | Base Oil; ASTM D445 |
| Evaporation Loss | 0.00 % | 0.00 % | 24 hrs, 100C; ASTM D972 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 250 | 250 | ASTM D217 |
| Penetration P(60), 1/10 mm | 271 | 271 | ASTM D217 |
| Oil Separation | 4.2 % | 4.2 % | 24 hrs, 100C; FTM 719B, 321.2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
| Pour Point | -67.0 °C | -88.6 °F | Base Oil; ASTM D97 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Base Fluid Type | PFPE(lin) | |
| Gellant Type | PTFE |