| Category | Polymer , Adhesive , Thermoset , Epoxy |
| Manufacturer | Abatron |
| Trade Name | AboCast |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Abatron AboCast 50-6/AboCure 50-12 Epoxy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 1.0 cP | 1.0 cP | 50-12 water-like viscosity |
| 4000 - 6000 cP | 4000 - 6000 cP | 50-6 | |
| 900 cP @Temperature 25.0 °C |
900 cP @Temperature 77.0 °F |
at 100/14 (50-6/50-12) pbw |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 107 | 107 | |
| Tensile Strength, Ultimate | 66.32 MPa | 9619 psi | |
| Elongation at Break | 4.4 % | 4.4 % | |
| Flexural Yield Strength | 107.49 MPa | 15590 psi | |
| Flexural Modulus | 2.785 GPa | 403.9 ksi | |
| Compressive Yield Strength | 109.21 MPa | 15840 psi | |
| Compressive Modulus | 1.81 GPa | 263 ksi | |
| Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 107 °C | 225 °F | Deflection temperature; load unknown. |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.29e+16 ohm-cm | 1.29e+16 ohm-cm | |
| Surface Resistance | 7.85e+14 ohm | 7.85e+14 ohm | |
| Dielectric Constant | 3.27 @Frequency 1e+6 Hz |
3.27 @Frequency 1e+6 Hz |
|
| 3.86 @Frequency 1000 Hz |
3.86 @Frequency 1000 Hz |
||
| 3.98 @Frequency 60 Hz |
3.98 @Frequency 60 Hz |
||
| Dissipation Factor | 0.010 @Frequency 60 Hz |
0.010 @Frequency 60 Hz |
|
| 0.027 @Frequency 1000 Hz |
0.027 @Frequency 1000 Hz |
||
| 0.031 @Frequency 1e+6 Hz |
0.031 @Frequency 1e+6 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Pot Life | 43 min | 43 min | 500 g |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Exotherm | 283°C | Peak |