| Category | Fluid , Lubricant , PTFE Gellant , Synthetic Ether Base |
| Manufacturer | Nye Lubricants |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nye Lubricants 856 (FG) Synthetic Oil.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity Measurement | 133 | 133 | Viscosity Index of Base Oil; ASTM D2270 |
| Kinematic Viscosity at 40°C (104°F) | 11 cSt | 11 cSt | Base Oil; ASTM D445 |
| Kinematic Viscosity at 100°C (212°F) | 3.0 cSt | 3.0 cSt | Base Oil; ASTM D445 |
| Evaporation Loss | 0.20 % | 0.20 % | 24 hrs, 100C; ASTM D972 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 280 | 280 | ASTM D217 |
| Penetration P(60), 1/10 mm | 265 | 265 | ASTM D217 |
| Oil Separation | 2.3 % | 2.3 % | 24 hrs, 100C; FTM 719B, 321.2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 150 °C | 302 °F | Recommended |
| Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | Recommended |
| Pour Point | -70.0 °C | -94.0 °F | Base Oil; ASTM D97 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Base Fluid Type | Ester(Di) | |
| Gellant Type | PTFE |