Material Notes:
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Information provided by Noble Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Melt Flow 14.84 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14.84 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength at Break 9.65 MPa
1400 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
2% Secant Modulus 0.179 GPa
26.0 ksi
ASTM D790
Tear Strength 50.3 kN/m
287 pli
ASTM D624
Processing Properties Metric English Comments
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature