Westlake Epolene® C-15 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® C-15 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: Epolene C-15 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and to provide lubricity in rubber compounding. Coatings produced with Epolene C-15 exhibit high gloss, low moisture vapor transmission rates, grease resistance, and good heat seal ability.Key Attributes:Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR Excellent thermal stabilityLow colorMedium molecular weightUseful in color concentratesApplication/Uses: Automotive refinishAutomotiveBuilding and ConstructionHot Melt Adhesive Packaging Solvent borne AdhesivesWax Modification
Physical Properties Metric English Comments
Specific Gravity 0.906 g/cc
0.906 g/cc
Viscosity 3000 - 4800 cP

@Temperature 150 °C
3000 - 4800 cP

@Temperature 302 °F
542-111
Brookfield Viscosity 1800 cP

@Temperature 190 °C
1800 cP

@Temperature 374 °F
ASTM D3226
8950 cP

@Temperature 125 °C
8950 cP

@Temperature 257 °F
ASTM D3226
Molecular Weight 17000 g/mol
17000 g/mol
Thermal Properties Metric English Comments
Flash Point >= 343 °C
>= 649 °F
ASTM E136
Ring & Ball Softening Point 101 °C
214 °F
ASTM E28
Optical Properties Metric English Comments
Gardner Color Number <= 1.0
<= 1.0
542-130
Descriptive Properties Value Comments
Penetration Hardness 4 dmm
ASTM D5, Needle under 100-g load for 5s @ 25°C, tenths of mm