Nabaltec APYMAG® 30 Magnesium Hydroxide

Category Ceramic , Oxide , Magnesium Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Nabaltec GmbH
Trade Name APYMAG®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec APYMAG® 30 Magnesium Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these products is of growing importance.If processing temperatures exceed 200°C, APYMAG® should be used. It is preferable for applications which are very sensitive to processing parameters, like viscosity. When using in thermoplastics, good mechanical and flame retardancy can be achieved.
Physical Properties Metric English Comments
Brightness 90 %

@Wavelength 457 nm
90 %

@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 19 %
19 %
ml/100 g
Moisture Absorption at Equilibrium 0.50 %
0.50 %
Loss On Ignition 31.0 %

@Temperature 105 - 1000 °C
31.0 %

@Temperature 221 - 1830 °F
Particle Size 12 µm
12 µm
Median Grain Diameter
Specific Surface Area 3.0 m²/g
3.0 m²/g
BET
Component Elements Properties Metric English Comments
CaO 3.0 %
3.0 %
Fe2O3 0.70 %
0.70 %
Electrical Properties Metric English Comments
Electrical Resistivity 2857 ohm-cm
2857 ohm-cm
Processing Properties Metric English Comments
Processing Temperature <= 300 °C
<= 572 °F
Descriptive Properties Value Comments
Mg(OH)2 90
Sieve Analysis (%) 0.2
> 45 µm